MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Nickel Alloy; Superalloy

Material Notes: INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt-iron alloy with aluminum, chromium, and niobium additions. The alloy is of considerable interest to aircraft gas turbine engine designers and materials engineers for containment and clearance control components such as rings, casings, shrouds and seals for compressors, turbines and exhaust systems. The three-phase age hardenable alloy offers a range of improvements for these applications over alternative alloys.

Information Provided by Special Metals Corporation

Key Words: UNS R30783; AMS 5490
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.81 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 807 MPa
@Temperature 704 °C
 979 MPa
@Temperature 649 °C
 1034 MPa
@Temperature 538 °C
 1076 MPa
@Temperature 427 °C
 1194 MPa
@Temperature 21.0 °C
Tensile Strength, Yield 607 MPa
@Temperature 704 °C
 683 MPa
@Temperature 649 °C
 686 MPa
@Temperature 538 °C
 717 MPa
@Temperature 427 °C
 779 MPa
@Temperature 21.0 °C
Elongation at Break 24 %
@Temperature 21.0 °C
 25 %
@Temperature 427 °C
 25 %
@Temperature 538 °C
 28 %
@Temperature 649 °C
 39 %
@Temperature 704 °C
Reduction of Area 39 %
@Temperature 649 °C
 42 %
@Temperature 427 °C
 44 %
@Temperature 21.0 °C
 46 %
@Temperature 538 °C
 64 %
@Temperature 704 °C
Rupture Strength 30500 psi
@Temperature 704 °C,
Time 3.96e+6 sec
 43500 psi
@Temperature 704 °C,
Time 1.44e+6 sec
 82700 psi
@Temperature 593 °C,
Time 3.96e+7 sec
 100000 psi
@Temperature 593 °C,
Time 1.44e+6 sec
 100000 psi
@Temperature 538 °C,
Time 3.96e+7 sec
 131000 psi
@Temperature 538 °C,
Time 1.08e+6 sec
Modulus of Elasticity 128.7 GPa
@Temperature 927 °C
 152.5 GPa
@Temperature 704 °C
 163.8 GPa
@Temperature 538 °C
 171.3 GPa
@Temperature 316 °C
 175.5 GPa
@Temperature 93.0 °C
 177.3 GPa
@Temperature 21.0 °C
Poissons Ratio 0.29
@Temperature 927 °C
 0.30
@Temperature 538 °C
 0.30
@Temperature 704 °C
 0.31
@Temperature 21.0 °C
 0.31
@Temperature 93.0 °C
 0.32
@Temperature 316 °C
Shear Modulus 49.8 GPa
@Temperature 927 °C
 58.6 GPa
@Temperature 704 °C
 62.8 GPa
@Temperature 538 °C
 65.0 GPa
@Temperature 316 °C
 67.0 GPa
@Temperature 93.0 °C
 67.8 GPa
@Temperature 21.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.08 µm/m-°C
@Temperature 200 °C
 10.33 µm/m-°C
@Temperature 500 °C
 10.94 µm/m-°C
@Temperature 800 °C
 12.33 µm/m-°C
@Temperature 1100 °C
Specific Heat Capacity 0.455 J/g-°C
Thermal Conductivity 10.1 W/m-K
@Temperature 21.0 °C
Annealed
 11.4 W/m-K
@Temperature 93.0 °C
Annealed
 14.8 W/m-K
@Temperature 316 °C
Annealed
 22.0 W/m-K
@Temperature 649 °C
Annealed
Melting Point 1336 - 1407 °C
Solidus 1336 °C
Liquidus 1407 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.0 - 6.0 %
Boron, B 0.0030 - 0.012 %
Carbon, C <= 0.030 %
Chromium, Cr 2.5 - 3.5 %
Cobalt, Co 28.083 - 39.90 %Remainder
Copper, Cu <= 0.50 %
Iron, Fe 24 - 27 %
Manganese, Mn <= 0.50 %
Nickel, Ni 26 - 30 %
Niobium, Nb (Columbium, Cb) 2.5 - 3.5 %
Phosphorus, P <= 0.015 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.0050 %
Titanium, Ti 0.10 - 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chosun Refractories CUN-738 Nozzle Brick
Special Metals INCONEL® Alloy 718
Waspaloy B Nickel Superalloy
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
IN-738 Cast Nickel Superalloy

NINDA04 / 98895

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.