MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Westlake HIFOR Xtreme® SC74884 Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: HIFOR Xtreme® SC74884 is an enhanced hexene LLDPE designed for blown film extrusion applications requiring high strength and toughness. HIFOR Xtreme® SC74884 contains no slip or anti-block. This material is highly stabilized and contains process aid. This product has some 21 CFR clearances. Application/Uses: Blown film extrusion, Heavy Duty Films.

Information provided by Westlake Chemical Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.915 g/cc0.0331 lb/in³ASTM D1505
Melt Index of Compound 0.75 g/10 min0.75 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 700 %700 %ASTM D882
Film Elongation at Break, TD 950 %950 %ASTM D882
Dart Drop Test 750 g1.65 lbASTM D1709
Film Tensile Strength at Break, MD 52.4 MPa7600 psiASTM D882
Film Tensile Strength at Break, TD 34.5 MPa5000 psiASTM D882
1% Secant Modulus, MD 172 MPa25000 psiASTM D882
1% Secant Modulus, TD 193 MPa28000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003
Gloss 62 %62 %@ 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 221 °C400 - 430 °Fblown fim extrusion
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Testing formTypical film property as measured on 1.0 mil film from blow film extruder.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8843 / 222915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.