MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. For 700 hours' ageing at 132 °C and pressure of 2 bars in water glycol environment, impact properties are increased by 50% in comparison with standard glycol grade TECHNYL A218 V30 black 34NG.

Available in: Asia Pacific and Latin America

Product Applications: TECHNYL® A 218 G1 V30 BLACK 34N is particularly recommended for the injection molding of parts in permanent contact with cooling liquids in cars, such as: cooling and heating radiator systems, header tanks, thermostat components, inlet / outlet pipes. This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183/A
Water Absorption 0.80 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 195 MPaISO 527 Type 1A
Elongation at Break 3.0 %ISO 527 Type 1A
Tensile Modulus 10000 MPaISO 527 Type 1A
Flexural Strength 280 MPaISO 178
Flexural Modulus 9200 MPaISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 85.0 kJ/m²ISO 179/1eU
 55.0 kJ/m²
@Temperature 120 °C,
Time 720000 sec
after aging water/glycol; ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 6.00e+14 ohmIEC 60093
Dielectric Strength 34.0 kV/mmIEC 60243
Dissipation Factor 0.010IEC 60250
Comparative Tracking Index 500 VSolution A; IEC 60112
 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
1210
Oxygen Index 23 %ISO 4589
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 270 - 280 °C
Front Barrel Temperature 280 - 290 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY
BASF Ultramid® A3WG6 HRX BK 23591 30% Glass Filled PA66 (Dry)
BASF Petra® 110 BK-112 15% Glass Filled PET
Domo TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, Conditioned

PRHOD666 / 137897

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.