MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI ALLEN® 2145HG Medium Impact ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Sheet

Material Notes: ALLEN® 2145HG is a general purpose ABS that has medium impact strength and a good cost to performance ratio to other materials like painted metal, FRP, aluminum, and other thermoplastics.

ALLEN® 2145HG has been tested under laboratory conditions and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302).

Suggested Application:

  • Covers and Housings
  • Vehicle Interiors
  • Displays
  • Signs
Features:
  • Custom color matching
  • Good forming properties
  • Edge trim easily used in future orders
  • UV protective films available
  • High gloss finish

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Linear Mold Shrinkage 0.000400 - 0.00700 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 34.4 MPaASTM D638
Flexural Strength 55.1 MPaASTM D790
Flexural Modulus 1930 MPaASTM D790
Izod Impact, Notched 106 J/m
@Temperature -18.0 °C
ASTM D256
 213 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 90.5 °Cannealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Gloss 80.0 %60° Angle; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSEKIS558 / 325298

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.