MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.

Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.

Uses: Injection molding.

Availability: Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: RETPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.0040 cm/cmflex bar; ASTM D955
 0.0050 cm/cmdisc; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61 - 67
@Time 5.00 sec
ASTM D2240
Tensile Strength, Ultimate 32.0 MPaASTM D638
Elongation at Break 180 %ASTM D638
Tensile Modulus 1030 MPaASTM D638
Flexural Strength 28.0 MPaASTM D790
Flexural Modulus 830 MPaASTM D790
Izod Impact, Notched 0.640 J/cm
@Temperature -40.0 °C
ASTM D256
 9.60 J/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 221 °C
Middle Barrel Temperature 226 °C
Front Barrel Temperature 226 °C
Nozzle Temperature 232 °C
Melt Temperature 232 °C
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
Injection Pressure 69.0 - 103 MPa
 69.0 - 103 MPa
Hold Pressure 35.0 - 69.0 MPa
 35.0 - 69.0 MPa
Back Pressure 50.0 psi
 50.0 psi
Screw Speed 30 - 80 rpm
 30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient OnFlex™ U 5370A-E0077 Thermoplastic Elastomer (TPE)
Covestro Texin® DP7-1157 Thermoplastic Polyurethane + ABS Blend
Avient Versollan™ RU 2204X Thermoplastic Elastomer (TPE)
Avient Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE)
Avient Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE)

PNOVEON502 / 121393

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.