MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

LyondellBasell Microthene MU76300 Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Microthene G polyolefin powders are ground, irregularly-shaped particles for use in a broad range of specialty applications. Microthene G powders combine the properties of a polyolefin resin with a small ground particle size. Applications: Automotive Parts, Color Concentrates, Industrial, Interior Automotive Applications, Structural Parts.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.927 g/cc0.0335 lb/in³ASTM D1505
Particle Mesh Size 35 Mesh35 Meshirregular particle shape; LYB Method
Vinyl Acetate Content 9.0 %9.0 %LYB Method
Melt Index of Compound 10 g/10 min10 g/10 minASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D <= 47<= 47ASTM D2240
 42
@Time 15.0 sec
42
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 12.0 MPa1740 psiASTM D638
Elongation at Break 760 %760 %ASTM D638
Flexural Modulus 0.144 GPa20.9 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 95.1 °C203 °FASTM D3418
Vicat Softening Point 72.0 °C162 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Descriptive Properties
Processing MethodPowders

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tisan TISETILEN® Flame Retardant (V0) Polyethylene
ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE)
Dow Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating

PEQT7614 / 219251

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.