MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® L1930 30% Glass Bead Filled Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: Description: 30% milled glass fibers, medium-viscosity, heat-stabilized, with processing aid

Applications: Gear wheels, castors, pump parts, sliding bearings, parts of fittings

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA12,MHR,18-040,GD30
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccISO 1183
Moisture Absorption at Equilibrium 0.50 %
@Thickness 1.00 mm,
Temperature 23.0 °C
50% R.H.; ISO 62
Water Absorption at Saturation 1.1 %
@Thickness 1.00 mm
ISO 62
Linear Mold Shrinkage 0.0030 cm/cm127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse 0.0070 cm/cm127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaISO 527-1/2
Tensile Strength, Yield 69.0 MPaISO 527-1/2
Elongation at Break 10 %ISO 527-1/2
Elongation at Yield 4.0 %ISO 527-1/2
Tensile Modulus 4.00 GPaISO 527-1/2
Charpy Impact Unnotched 6.50 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
 7.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 1.10 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.4
@Frequency 1e+6 Hz
IEC 60250
 4.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 40.0 kV/mmK20/P50; IEC 60243-1
Dissipation Factor 0.024
@Frequency 1e+6 Hz
IEC 60250
 0.031
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 600 VTest Solution A, 50 drops; IEC 60112
 600 VTest Solution A, 100 drops; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
45x15x10 mm; ISO 11359
Melting Point 178 °CPeak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 170 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 130 °CISO 75
Vicat Softening Point 170 °C50N; ISO 306
 175 °C10N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Descriptive Properties
Electrolytic CorrosionA1 StepIEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® L1901 nf (dry properties) Nylon 12
Polyplastics Duracon® GH-25 Acetal Co-polymer (POM), GF 25% reinforced, High strength, High rigidity
Evonik Vestamid® L1833 30% Glass Filled Nylon 12
Evonik Vestamid® L-GF15 23% Glass Filled Nylon 12
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General

PHULA28 / 47388

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.