MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxies, Etc 50-1220 One Component Silicone Thermal Grease
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: 50-1220 is a one component thermal grease. This heavy filled Heat Sink Compound promotes high thermal conductivity, low bleed, and high temperature stability. The 50-1220 is engineered for applications requiring fast heat dissipation and electrical insulation. This one part silicone heat sink compound is available in 8 oz jars, 16 oz jars, and quarts. Special syringe packaging is available upon request.

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Penetration 245245Worked 1,000,000 strokes
 275275Worked 60 strokes
 300300Unworked
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cm
Dielectric Constant 5.0
@Frequency 100 Hz
5.0
@Frequency 100 Hz
Dielectric Strength 8.27 kV/mm210 kV/in
Dissipation Factor 0.010
@Frequency 100 Hz
0.010
@Frequency 100 Hz
Arc Resistance 160 sec160 sec
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.15 W/m-K7.98 BTU-in/hr-ft²-°F
 
Descriptive Properties
Bleed0.0005after 24 hours @ 200°C
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX041 / 316718

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.