MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled
Categories: Polymer; Thermoplastic; Polystyrene (PS); Syndiotactic Polystyrene (SPS); Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber

Material Notes: Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/cc
Filler Content 30 %
Moisture Absorption 0.010 %24 hrs., 50% RH
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm
Linear Mold Shrinkage, Transverse 0.0030 - 0.0070 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPa
Elongation at Break 2.3 %
Tensile Modulus 9.10 GPa
Flexural Yield Strength 185 MPa
Flexural Modulus 8.90 GPa
Izod Impact, Notched (ISO) 13.0 kJ/m²
Izod Impact, Unnotched (ISO) 41.0 kJ/m²
Charpy Impact Unnotched 50.0 kJ/m²
Charpy Impact, Notched 14.0 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cm
Dielectric Constant 3.1
Dielectric Strength 28.0 kV/mmASTM D145
Dissipation Factor 0.0010IEC 60250
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 250 - 400 VIEC 60112
Hot Wire Ignition, HWI >= 120 sec
@Thickness 1.50 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/minUL746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 23.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
CTE, linear, Transverse to Flow 49.0 µm/m-°C
Deflection Temperature at 0.46 MPa (66 psi) 265 °C
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
UL RTI, Electrical 110 °CUL746B
UL RTI, Mechanical with Impact 110 °CUL746B
UL RTI, Mechanical without Impact 110 °CUL746B
Flammability, UL94 HB
@Thickness 0.750 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 310 °C
Mold Temperature 50.0 - 80.0 °C
 130 - 155 °CFor optimal surface finish
 
Descriptive Properties
CommentsISO10993
 NSF61

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Idemitsu Kosan Xarec® EA 522 SPS, 22% Glass Filled
Idemitsu Kosan Xarec® WA 214 SPS, 40% Glass Filled
Idemitsu Kosan Xarec® WA 214LG SPS, 40% Glass Filled
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled
Idemitsu Kosan Xarec® EA 513 SPS, 30% Glass Filled

PIDEM113 / 150220

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.