MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay MIRATAINE® CAB AS Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Cocamidopropyl Betaine (30% solids). Foam boosters, foaming agents, thickeners and conditioners. Compatible with anionic surfactants and most cationic polymers. Glycerine free

Chemical Name: COCAMIDOPROPYL BETAINE

CAS: 70851-07-9

Available in: North America

Applications: Mirataine CAB AS is an amphoteric surfactant that imparts mildness to shampoo & skin cleanser products. Mirataine CAB AS will boost foam and aid in formulation viscosity. Mirataine CAB AS is stable over a wide pH range and is compatible with anionic surfactants and most cationic polymers.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 4.0 - 5.54.0 - 5.55% in DW; RP-0420
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 61 - 65 %61 - 65 %RP-0327
 
Descriptive Properties
AppearanceClear, slightly yellow
Assay29-31%
Color<200APHA, RP-0134
CompositionFree Amidoamine<0.5%, RP-1326
 Free Coconut Fatty Acid<0.5%
 Microorganisms<500 cfu/ml, RP-1370
 Sodium Chloride4.5-6%, RP-0097
 Sodium Glycolate<0.7%, RP-0108
 Total Chloroacetic Acids<150
Foreign MatterFree of foreign material

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tenite Acetate 109E3V46022 Natural, Trsp Cellulose Acetate
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate
Daikin NEOFLON® EP-521 Extrusion Grade ETFE
Chemours Tefzel® 207 Resin Modified ETFE

WRHOD283 / 137514

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.