MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt Silvaloy® 559 Silver Based Cadmium Free Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Braze 559 is an intermediate temperature silver brazing alloy similar to Braze 541 (54 Ag, 40Cu, 5 Zn, 1 Ni). It has a rather long melting range (220EF/105EC) so that it will tend to liquate (i.e. separate high from low melting phases) if it is heated slowly through its melting range. However, the long melting range is useful when wide gap joints are brazed as it will bridge the gap and produce larger fillets than alloys with short melting ranges that are more fluid. For torch brazing or furnace brazing with flux it is recommended that Handy Flux type B-1 be used with this alloy.

Applications:Although Braze 559 may be used in flux type brazing, its principal use has been in fluxless brazing of stainless steels in dry hydrogen atmosphere. Braze 559 is free of zinc and it would have an advantage over Braze 541 in fluxless furnace brazing applications where zinc volatilization is objectionable.

Specifications: Braze 559 conforms to the following specifications-AWS A5.8 BAg-13a, ASME Boiler & Pressure Vessel Code Sec. II C SFA-5.8 BAg-13a, SAE AMS 4765

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.75 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000337 ohm-cmHard
 
Thermal PropertiesOriginal ValueComments
Melting Point 1420 - 1640 °F
Solidus 1420 °FMelting Point
Liquidus 1640 °FFlow Point
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 40.35 %
Nickel, Ni 1.5 - 2.5 %
Other, total <= 0.15 %
Silver, Ag 56 - 57 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMW® ELKONIUM 18 silver, copper, cadmium alloy
NAECO® ELKONIUM® 43 palladium based alloy
NAECO® ELKONIUM® 63 Silver Alloy
Johnson Matthey Argo-braze™ 562 Silver Brazing Filler Metal
CMW® ELKONIUM 63 Silver Alloy

NLUCMI24 / 18091

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.