MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SCG Chemicals M735RW Linear low density polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: SCG M735RW is a linear-low density polyethylene (LLDPE) for rotational molding applications. M735RW is a natural color PE resin available in a pellet and powder form, whereas M70 is the color compound version. With a high melt flow and a balance of impact strength, stiffness, and process ability, this grade is suitable for rotational molding of lawn and garden articles, decorative items, and small industrial parts.

Applications: Lawn and garden articles, Decorative items, LED lamp covers, Small industrial parts , Intricate automotive articles.

Features: High melt flow suitable for complex shape. Superior gloss and surface finish. Smooth inside surface. UV8 for outdoor use. Good rigidity and toughness.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.932 g/ccASTM D 1505
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57ASTM D2240
Tensile Strength at Break 21.0 MPaCrosshead speed 50 mm/min.; ASTM D638
Tensile Strength, Yield 17.0 MPaCrosshead speed 50 mm/min.; ASTM D638
Elongation at Break 1000 %Crosshead speed 50 mm/min; ASTM D638
Flexural Modulus 570 MPaASTM D790
Impact 25
@Thickness 5.50 mm,
Temperature -40.0 °C
J/mm ARM Method, rotomolded
 
Thermal PropertiesOriginal ValueComments
Melting Point 125 °CASTM D2117
Crystallization Temperature 113 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 58.0 °CASTM D648
Vicat Softening Point 108 °CASTM D1525
Brittleness Temperature <= -60.0 °CASTM D746
 
Descriptive Properties
AppearanceColored compound pellet
 Colored compound powder
 Natural Pellet
 Natural Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC743 / 278000

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.