MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 7714A Epoxy - Unidirectional Carbon Tape and Roving Composite
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: CYCOM® 7714A resin is a 250°F (121°C) curing epoxy resin with 160°F (71°C) wet service temperature capability. CYCOM 7714A is formulated for autoclave processing but has been successfully processed by press molding. Unidirectional tape and woven fabric impregnated with CYCOM 7714A resin will retain excellent tack and drape for at least 10 days at 72°F (22°C). Standard cure cycle is two hours at 250°F (121°C). No post cure is required for 160°F (71°C) wet service capability. CYCOM 7714A can be impregnated via solution and hot melt techniques on all available fibers and fabrics.

Features & Benefits:

  • 250°F (121°C) cure
  • Available on fabric, tape and roving
  • Large industry database
  • Flame retardant
  • 200°F (93°C) dry service temperature
  • 160°F (71°C) wet service temperature
  • Laminate and sandwich panel usage
  • Autoclave and press mold processing
  • Used as self-adhesive system
  • Co-curable with CYCOM 7701, CYCOM 7714 and CYCOM 97714A resins
  • Meets all NASA outgassing requirements
  • Shelf life of 6 months at 0°F (-18°C), 10 days at 72°F (22°C)
Applications:
  • Aircraft interiors
  • Seats and control surfaces
  • UAV and secondary structure
Property data reported for epoxy 7714a reinforced with 57-63% fiber volume Unidirectional Tape and Roving, Standard Modulus Carbon Fiber [33Msi (228 GPa).

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 - 1.26 g/ccCured Resin
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 230000 - 320000 psi
@Temperature 71.0 °C
 260000 - 300000 psi
@Temperature -54.0 °C
 260000 - 350000 psi
@Temperature 24.0 °C
Elongation at Break 0.95 - 1.25 %
@Temperature -54.0 °C
 1.05 - 1.35 %
@Temperature 24.0 °C
 1.05 - 1.35 %
@Temperature 71.0 °C
Tensile Modulus 103 - 152 GPa
@Temperature -54.0 °C
 110 - 145 GPa
@Temperature 24.0 °C
 97.0 - 159 GPa
@Temperature 71.0 °C
Flexural Strength 218000 - 266000 psi
@Temperature 24.0 °C
Flexural Modulus 97.0 - 117 GPa
@Temperature 24.0 °C
Compressive Strength 745 - 1379 MPa
@Temperature 71.0 °C
 1172 - 1655 MPa
@Temperature 24.0 °C
Compressive Modulus 76000 - 138000 MPa
@Temperature 24.0 °C
Shear Strength 7000 - 11000 psi
@Thickness 1800 mm
Interlaminar
 11000 - 13000 psi
@Thickness 610 mm
Interlaminar
 13000 - 17000 psi
@Thickness -1370 mm
Interlaminar
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 71.0 °Cwet
 93.0 °Cdry
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 °F
@Time 7200 sec
Standard Cure
Shelf Life 0.333 Month
@Temperature 22.2 °C
 6.00 Month
@Temperature -17.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Hysol Benzoxazine 99110 Infusion Resin
Solvay CYCOM® 977-3 Neat Epoxy Resin
Solvay CYCOM® 7714 Epoxy Resin
Solvay CYCOM® 970 Epoxy - Carbon Fiber Reinforced Unidirectional Tape
Solvay CYCOM® 7668 Epoxy Resin

PCYTED085 / 180387

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.