Formolene® HP4525 is a high performance copolymer designed for non-pressure pipe applications. It has good long-term hoop strength performance and outstanding toughness even at low temperatures. It provides an excellent balance of stiffness, and processability in conduit pipe applications. Formolene HP4525 meets the requirements of ASTM F2160, UL651A and NEMA TC-7. DP4525A also meets a minimum ASTM D3350 Cell Classification of 335430A. Suggested Applications: Conduit Pipe, Telecommunications Pipe, Drip Irrigation Pipe. Information provided by Formosa Plastics. |