MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Ateva® 1081 Film Ethylene Vinyl Acetate Copolymer Film
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Ateva® 1081 resin is well suited for film extrusion requiring superior sealability and strength. This EVA resin may be safely used as articles or components of articles intended for uses in contact with food as provided in FDA regulation 21 CFR 177.1350 - Ethylene-vinyl acetate copolymers, subject to extraction limitations on the finished food-contact article as specified in that regulation. This polymer may be processed on conventional extrusion equipment. It is recommended that the melt temperature be kept below 210°C as decomposition can occur at higher temperatures. Properties listed are for a film produced on a 24:1 L/D, 40 mm extruder with a 100 mm die, at a melting temperature of 210°C. Additives:

Applications: Flexible Packaging

Information provided by Celanese Corporation.

Key Words: film extrusion requiring superior sealability and strength
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.933 g/ccASTM D1505; ASTM D1928 Proc A
Vinyl Acetate Content 9.0 %AT Plastics PTM-39
Thickness 75.0 microns
Melt Flow 1.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 8.00 MPaMethod A (500 mm/min); ASTM D882
Film Tensile Strength at Yield, TD 7.00 MPaMethod A (500 mm/min); ASTM D882
Film Elongation at Break, MD 380 %Method A (500 mm/min); ASTM D882
Film Elongation at Break, TD 550 %Method A (500 mm/min); ASTM D882
Dart Drop 5.00 g/micronf50; ASTM D1709
Film Tensile Strength at Break, MD 23.0 MPaMethod A (500 mm/min); ASTM D882
Film Tensile Strength at Break, TD 24.0 MPaMethod A (500 mm/min); ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 102 °CDSC; ASTM D3417
Vicat Softening Point 82.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 20 %ASTM D1003
Gloss 34 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Blow-up Ratio (BUR) 2.1
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade
Celanese Ateva® 1081 Ethylene Vinyl Acetate Copolymer
Arkema Evatane® 1020 VG 5 Ethylene Vinyl Acetate
Celanese Ateva® 1221 Film Ethylene Vinyl Acetate Copolymer Film
Arkema Evatane® 1006 VL 2E Ethylene Vinyl Acetate

PATEVB39 / 25995

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.