MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Crucible Steel 446 Chromium Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.65 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 170
Tensile Strength, Ultimate 80000 psi
 2500 psi
@Temperature 1040 °C
 17000 psi
@Temperature 704 °C
Tensile Strength, Yield 50000 psi
@Strain 0.2 %
Elongation at Break 25 %in 2"
Reduction of Area 45 %
Creep Strength 2.068 MPa
@Temperature 816 °C
0.0001% per hour
 41.37 MPa
@Temperature 538 °C,
Time 3.60e+7 sec
Creep rate: 0.0001% per hour
Rupture Strength 3.447 MPa
@Temperature 871 °C,
Time 3.60e+6 sec
 5.516 MPa
@Temperature 871 °C,
Time 3.60e+6 sec
 20.68 MPa
@Temperature 593 °C,
Time 3.60e+7 sec
 38.61 MPa
@Temperature 593 °C,
Time 3.60e+6 sec
Modulus of Elasticity 29000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000670 ohm-cm
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.80 µin/in-°F
@Temperature 0.000 - 100 °C
 6.70 µin/in-°F
@Temperature 0.000 - 982 °C
Specific Heat Capacity 0.120 BTU/lb-°F
@Temperature 0.000 - 100 °C
Thermal Conductivity 145.2 BTU-in/hr-ft²-°F
@Temperature 93.3 °C
 169.2 BTU-in/hr-ft²-°F
@Temperature 538 °C
Melting Point 2600 - 2750 °F
Solidus 2600 °F
Liquidus 2750 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.20 %
Chromium, Cr 23 - 27 %
Iron, Fe >= 69.98 %As Remainder
Manganese, Mn <= 1.5 %
Nitrogen, N <= 0.25 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel 18 SR® Ferritic Stainless steel
AISI Type S14800 Stainless Steel condition SRH1050
AISI Type S14800 Stainless Steel condition A
AISI Type H13 Hot Work Tool Steel
AISI 1035 Steel, as rolled, 19-32 mm (0.75-1.25 in) round

NCRUC050 / 16043

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.