MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ascend Performance Materials Vydyne® A 30 GF BK EST KW2 UV PA66-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Vydyne A 30 GF BK EST KW2 UV is standard flow, organic heat stabilized, 30% glass-fiber reinforced PA66 resin. Available in black, this product is also lubricated for improved machine feed and flow and it is UV stabilized for outdoor applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³DAM; ISO 1183
Moisture Absorption at Equilibrium 1.7 %1.7 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 2.00 mm
0.0030 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
@Thickness 2.00 mm
0.0070 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psi50% RH; ISO 527-2
 175 MPa25400 psiDAM; ISO 527-2
Elongation at Break 2.0 %2.0 %DAM; ISO 527-2
 4.5 %4.5 %50% RH; ISO 527-2
Tensile Modulus 6.80 GPa986 ksi50% RH; ISO 527-2
 9.50 GPa1380 ksiDAM; ISO 527-2
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 575 V
@Thickness 3.00 mm
575 V
@Thickness 0.118 in
IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FUnannealed; DAM; ISO 75-2/A
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 265 - 295 °C509 - 563 °FInjection
Middle Barrel Temperature 265 - 295 °C509 - 563 °FInjection
Front Barrel Temperature 265 - 295 °C509 - 563 °FInjection
Nozzle Temperature 265 - 295 °C509 - 563 °FInjection
Melt Temperature 265 - 295 °C509 - 563 °FInjection
Mold Temperature 70.0 - 90.0 °C158 - 194 °FInjection
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection
Dry Time >= 3.00 hour>= 3.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
AppearanceBlack
FeaturesChemical Resistant
 Gasoline Resistant
 General Purpose
 Good Flow
 Good Heat Resistance
 Lubricated
 Organic Heat Stabilized
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9251 / 287604

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.