MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGOPREN® 6814 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: TEGOPREN® 6814 is an alkyl modified siloxane (liquid silicone wax) of organophilic behavior.

Application: TEGOPREN® 6814 can be used as an additive for thermoplastic polymer formulations to improve lubrication and surface slip properties. In textile application it can be used as an additive for fiber finishing to improve lubrication or wetting and spreading of non-polar systems. TEGOPREN® 6814 can also be used as an additive in softener formulations to improve the smooth hand of fabrics.

Benefits: TEGOPREN® 6814 shows the following benefits due to its capability to combine the properties of the organic modification and those of siloxanes:

  • improve mold release properties during injection molding which allows faster cycle times and less machine down time
  • improved flow characteristics which will finally result in the reduction of amperage values and lower energy consumption
  • better processability resulting in higher through-put
  • higher surface quality giving better water repellency, surface gloss and lower friction
  • Reduction of fiber and fiber metal friction.
  • Improved hand of softener formulations

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/cc
Viscosity 350 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 100 °C
 
Descriptive Properties
Appearanceliquid, colorless to pale straw
Content100%Active matter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGOPREN® 5847 Additive
Evonik TEGO® Antifoam 2290 Antifoam concentrate
Evonik TEGOPREN® 5851 Defoamer
Evonik TEGOPREN® 5852 Additive
Evonik TEGOPREN® 5863 Defoamer

PEVONIL604 / 196808

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.