MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets
Categories: Polymer; Thermoplastic; Polyurethane, TP; Silicone Polyurethane, Ether Based

Material Notes: Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc. Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight >= 95000 g/molMn by GPC using polystyrene stds; TM-005
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60 - 70TM-025
Tensile Strength at Break 25.0 - 42.0 MPaTM-019G
Tensile Stress at Strain 23.0 MPa
@Strain 100 %
Elongation at Break >= 200 %TM-019G
Modulus of Elasticity 0.550 - 0.750 GPaTM-019E
 
Thermal PropertiesOriginal ValueComments
Melting Point 175 - 195 °CDSC Induction Temperature; TM-029
 
Descriptive Properties
Polydispersity1.5-2.2TM-005; Mw/Mn by GPC using polystyrene stds

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets

PAORT904 / 107029

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.