MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Gougeon Brothers PRO-SET® ADV-175/ADV-273 Adhesive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Shear thinning resins and hardeners are thixotropic gels. The mixture fills gaps and will not sag on vertical surfaces. The material wets out the substrate, making priming or pre-wetting unnecessary on most surfaces, while ensuring a good bond.
Fast cure speed hardener provides approximately 20 minutes of working time at 72°F (22°C).
Room temperature cure properties suitable for many composite components and structures.
High performance pre-thickened, two-part epoxy adhesives for secondary bonding of laminated composites, steel, aluminum, cast iron, concrete, stone, and most wood species. PRO-SET Adhesives will bond these materials, to one another in any combination.
Coverage one cartridge set dispenses approximately 47 ft of 1/4" bead, or 17 ft of 1/2" bead and will cover approximately 7 sq ft when spread with a 1/8" x 1/8" notched spreader, or 12 sq ft with a 1/16" x 1/16" notched spreader.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccHardener
 1.17 g/ccResin
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D2240
Tensile Strength 6250 psi
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D638
Elongation at Break 4.2 %
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D638
Tensile Modulus 380000 psiASTM D638
Flexural Strength 11100 psi
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D790
Flexural Modulus 370000 psi
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D790
Compressive Yield Strength 10700 psi
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D695
Shear Strength 1830 psion 2024T Aluminum; ASTM D1002
 2280 psion 1018 Steel; ASTM D1002
Adhesive Bond Strength 1420 psito 2024T Aluminum; ASTM D4541
 2540 psito 1018 Steel; ASTM D4541
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 113 °F
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
ASTM D648
Glass Transition Temp, Tg 122 °F
@Treatment Temp. 22.0 °C,
Time 1.21e+6 sec
DSC Onset– 1st Heat; ASTM E1356
 
Processing PropertiesOriginal ValueComments
Pot Life 18.0 - 22.0 min
@Temperature >=7.00 °C
1/2" bead; ASTM D2471
 9.00 - 11.0 min
@Load 0.100 kg
ASTM D2471
Shelf Life 18.0 Monthresin
 18.0 Monthhardener
 
Descriptive Properties
Mix ratio100:47.2Weight, Resin: Hardener
 100:50.0Volume, Resin: Hardener
 2.00:1Volume, Resin: Hardener
 2.12:1Weight, Resin: Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOUGP939 / 290782

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.