MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik TEGOPREN® 5840 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: TEGOPREN® 5840 is a polyether siloxane. It is a non-ionic product with 100 % active content.

Application: Apart from its extraordinary reduction of surface tension in aqueous solutions, the main property of TEGOPREN® 5840 is super spreading. This is the fast coverage of large hydrophobic surfaces. TEGOPREN® 5840 is advisable in a multitude of industrial applications where negative interaction between substrates and coatings has to be overcome TEGOPREN® 5840 shows excellent surface wetting in adhesive applications, where the coating of difficult substrates is required. Therefore, it is recommended for the production of transfer labels and tapes or for laminating processes. Furthermore, it is suitable for sealant applications

Benefits: TEGOPREN® 5840 is a solvent free easy to handle liquid. Due to its non-ionic nature it is compatible with cationic, anionic, non-ionic and amphoteric surfactants. The use of small amounts of TEGOPREN® 5840 reduces the surface tension of water based systems. It therefore enhances the spreading on non-polar surfaces e. g. polypropylene. Due to the special selection of active ingredients TEGOPREN® 5840 might outperform, depending on the formulation and application, conventional wetting agents such as sulfosuccinates in foam (inhibiting) behaviour. TEGOPREN® 5840 improves spreading and wetting properties (e. g. in metal working fluids)

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 40 - 90 cP
Surface Tension 22 dynes/cm0.1% in water
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 101 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.443 - 1.451
 
Descriptive Properties
Appearanceliquid, colorless to pale straw
Cloud point20-30°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGO® Antifoam 2290 Antifoam concentrate
Evonik TEGOPREN® 5851 Defoamer
Evonik TEGOPREN® 5847 Additive
Evonik TEGOPREN® 5852 Additive
Evonik TEGOPREN® 5863 Defoamer

PEVONIL595 / 196799

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.