MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ChevronTexaco 100 Aircraft Engine Oils Premium AD
Categories: Fluid; Lubricant

Material Notes: Texaco Aircraft Engine Oils Premium AD deliver value through:
  • Clean engines due to the dispersancy action. Minimal deposits in the combustion chamber, spark plugs, rings, valves, etc.
  • Low wear — Maximum parts life by resisting corrosion and deposits from oil oxidation
  • Rigid quality control throughout the production process
  • Early starting at low temperatures and stable viscosity grade over a wide temperature range.

Texaco Aircraft Engine Oils Premium AD are premium quality ashless dispersant oils for four-stroke aircraft piston engines.

Texaco Aircraft Engine Oils Premium AD are blended with high quality, high viscosity index base oils, ashless dispersant additives, and antioxidant, and antifoam agents.

The ashless dispersant additives retard the formation of sludge and varnish without forming harmful ash deposits in the combustion chamber. The antioxidants resist oxidation, which causes oil thickening and corrosion. The antifoam agent is used to prevent oil foam formation, which can cause unstable oil pressure and loss of film strength.

Texaco Aircraft Engine Oils Premium AD are recommended for use in all makes of piston aircraft engines in single and multi-engine light planes and transport type aircraft.

Texaco Aircraft Engine Oils Premium AD meet all specification requirements of:

  • Textron Lycoming Specification 301F
  • Teledyne Continental Motors Specification MHS-24
  • Pratt & Whitney Service Bulletin #1183T

Texaco Aircraft Engine Oils Premium AD meet the requirement of SAE J1899, which has replaced MIL-L-22851D as the standard of nondispersant oils.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 221684; MSDS Number: 8623

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 29.1 °
Viscosity Measurement 117Viscosity Index
Kinematic Viscosity at 40°C (104°F) 181 cSt
Kinematic Viscosity at 100°C (212°F) 18.8 cSt
Ash 0.00 %Sulfated Ash
 
Thermal PropertiesOriginal ValueComments
Pour Point -27.0 °C
Flash Point 248 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 1410 ANTIFOAM
ChevronTexaco AFP White Oil
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil Uncompounded
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil AD
ChevronTexaco Aero 50/Grade 100 Engine Oil AD Uncompounded

WTEXA002 / 76881

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.