Description: Conoco Syncon HP Synthetic Grease is a high-quality, synthetic polyalphaolefin (PAO) lithium grease developed to provide exceptional protection and corrosion resistance for bearings and moving parts operating in corrosive environments at moderate to arctic temperatures. It flows readily to lubricate the idler bearings in extended-length conveyors, the chassis and wheel bearings of on- and off-road equipment and other applications where low-temperature pumpability and fluidity are critical. Conoco customers have successfully used this product to lubricate equipment operating at temperatures as low as -55°F (-48°C) using conventional and air-operated grease guns. Syncon HP Synthetic Grease is approved by General Motors Corporation under part No. 9985377 to lubricate the moving mechanisms for automobile seats and shifters during assembly operation. Information provided by ConocoPhillips. Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012. |