One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose for bonding metals, plastics, and glass. Data provided by the manufacturer, GE Silicones. GE Silicones became a part of Momentive Performance Materials in 2006. |
RTV Silicones; R.T.V. Silicones |