MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Lucalen A2700P LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Lucalen A2700P is a low density polyethylene, containing butyl acrylate comonomer. It exhibits low stiffness, low hardness and good impact properties at low temperature. Lucalen A2700P is suitable for industrial applications where a combination of good processability and excellent softness is required. It is compatible with other Lucalen grades and is miscible with other ethylene copolymers, PE-LD, PE-HD and PE-LLD. The grade is available in natural pellet form. This grade is not intended for medical and pharmaceutical applications.

Availability: Asia-Pacific; Europe

Application: Bitumen Modification; Polymer Modifier; Soft Profile & Sheets; TPO Foils and Skins; Wire & Cable

Market: Compounding; Industrial, Building & Construction

Processing Method: Cast Film; Compounding; Extrusion Coating; Injection Molding

Attribute: Good Adhesion; Good Chemical Resistance; Good ESCR (Environmental Stress Cracking Resistance); Good Optical Properties; Good Processability; High Filler Loading Capability; High Flow; Low Temperature Flexibility; Low Temperature Impact Resistance; Soft

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ISO 1183-1
Melt Flow 15.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
15.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 29.029.0ISO 868
Tensile Strength at Break 9.00 MPa1310 psiISO 527-1, -2
Elongation at Break 600 %600 %ISO 527-1, -2
Flexural Modulus 0.0400 GPa5.80 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 93.0 °C199 °FPeak; ISO 11357-3
Vicat Softening Point 55.0 °C131 °FA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9644 / 324579

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.