MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
LyondellBasell Montell 1900H UHMW Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes:
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, FDA acceptable

Applications: wear surfaces in pulp and paper process, material handling and packaging equipment, food and beverage processing systems, impact and abrasion resistant parts for mining and solid waste handling, marine fendering, battery separators

Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.

Description: 1900H ultrahigh molecular wight polyethylene resin has an average molecular weight range between 4 and 6 million. This polymer is for use in compression moldind, solution and ram extrusion processes. It is supplied in a fine powder form. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All indgredients meet the chemical regristration requirments of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792
Apparent Bulk Density 0.470 - 0.470 g/ccASTM D792
Viscosity Test 2900 cm³/gIntrinsic; ASTM D4020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 68ASTM D2240
Tensile Strength, Ultimate 40.0 MPaASTM D638
Tensile Strength, Yield 19.0 MPaASTM D638
Elongation at Break 310 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Flexural Modulus, 1% Secant 0.750 GPa0.05 in/min; ASTM D790B
Izod Impact, Notched NBASTM D256
Abrasion 7.7% Abrasion Index; Montell P116 Test
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Plastics Lennite® GUR1020 (Type I) UHMW-PE For Medical Applications
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE
Polikim ULPOLEN® 1000 UHMWPE Standard
Westlake Plastics Lennite® GUR1050 (Type II) UHMW-PE For Medical Applications
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)

PMO570 / 53679

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.