MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Go Yen Chemical GY-FR-202H Non-halogen Plastics Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Features: Excellent Fire Resistant Effect, Can reduce smoking, Not easy to affect end-product physical property, halogen free.

Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD is the largest manufacturer of flame retardant in Taiwan. We have nearly 40 years of experience developing functional additives and providing a series of solutions for general plastic and engineering plastic industry.

Advantages:

  • Excellent Fire Resistant Effect
  • Can reduce smoking
  • Not easy to affect end-products physicals’ property
  • Non halogen
  • High Pyrolysis
  • Non-Toxic
Applications: Engineering Plastics, Epoxy Industrial (Resin/CCL/EMC), Rubber flame retardant plasticizer, Other Application etc.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 354 °C669 °F
Decomposition Temperature >= 270 °C>= 518 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 1.0 %<= 1.0 %
 
Descriptive Properties
AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN022 / 266330

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.