MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Monprene® CP-19234 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-19234 is a general purpose thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-19234 is a low hardness, low density grade that is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Flexibility; Good Processability; Low Density; Low Hardness; Soft

Uses: Closures; Consumer Applications; Gaskets; Handles; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.882 g/cc0.0319 lb/in³ASTM D792
Melt Flow 23 g/10 min
@Load 2.16 kg,
Temperature 190 °C
23 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3737ASTM D2240
Tensile Strength at Break 5.00 MPa725 psiASTM D412
Elongation at Break 600 %600 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 199 - 249 °C390 - 480 °FMelt, Injection
Rear Barrel Temperature 182 - 232 °C360 - 450 °FInjection
Middle Barrel Temperature 188 - 238 °C370 - 460 °FInjection
Front Barrel Temperature 193 - 243 °C380 - 470 °FInjection
Nozzle Temperature 199 - 249 °C390 - 480 °FInjection
Zone 1 182 - 232 °C360 - 450 °FExtrusion
Zone 2 188 - 238 °C370 - 460 °FExtrusion
Zone 3 193 - 243 °C380 - 470 °FExtrusion
Zone 4 193 - 243 °C380 - 470 °FExtrusion
Zone 5 199 - 249 °C390 - 480 °FExtrusion
Die Temperature 199 - 249 °C390 - 480 °FExtrusion
Mold Temperature 35.0 - 48.9 °C95.0 - 120 °FInjection
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0807 / 237298

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.