MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC SABIC® HDPE ICP4907S PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: SABIC® HDPE ICP4907S is part of SABIC's high density polyethylene Industrial Container Product portfolio. SABIC® HDPE ICP4907S is typically used for state of the art blow molding UN certified Intermediate Bulk Containers and Heating Oil Tanks, up to 1000 liters and more. This UV-stabilized and food approved grade combines good processing performance with good stress crack resistance, stiffness and impact performance. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccCompression moulding of test specimen according to ISO 1872-2; ASTM D1505
Environmental Stress Crack Resistance 30 hourISO 18488
ESCR 10% Igepal® 800 hourCO-630, F50; ASTM D1693B
Melt Flow 7.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ISO 868
Tensile Strength at Break 34.0 MPaSpeed of testing: 50 mm/min,Test specimen according to ISO 527-2 type 1BA, thickness 2 mm; ISO 527-2
Tensile Strength, Yield 23.0 MPaSpeed of testing: 50 mm/min,Test specimen according to ISO 527-2 type 1BA, thickness 2 mm; ISO 527-2
Elongation at Break 1000 %Speed of testing: 50 mm/min,Test specimen according to ISO 527-2 type 1BA, thickness 2 mm; ISO 527-2
Tensile Modulus 950 MPaSpeed of testing: 50 mm/min,Test specimen according to ISO 527-2 type 1BA, thickness 2 mm; ISO 527-2
Flexural Strength 24.0 MPaISO 178
Flexural Modulus 1000 MPaISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 192 J/gISO 11357-3
Melting Point 131 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °CConditioning of test specimen: temp. 23 °C, relative humidity 50 %, 24 hours; ISO 75-2
Vicat Softening Point 126 °Cat 10 N (VST/A); ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10914 / 244381

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.