MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.

Information provided by Firestone

Key Words: PA6; Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccASTM D792
Linear Mold Shrinkage 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 160 MPaASTM D638
Elongation at Break 3.5 %ASTM D638
Flexural Yield Strength 205 MPaASTM D790
Flexural Modulus 8.30 GPaASTM D790
Izod Impact, Notched 1.20 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.6 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Melting Point 220 °C
Deflection Temperature at 0.46 MPa (66 psi) 216 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 520 - 540 °F
Middle Barrel Temperature 530 - 550 °F
Front Barrel Temperature 510 - 530 °F
Nozzle Temperature 500 - 520 °F
Melt Temperature 520 - 540 °F
Mold Temperature 130 - 180 °F
Drying Temperature 165 °F
Dry Time 4 hour
Moisture Content <= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient OnForce™ LFT NN-30 LCF/000 Natural Nylon 66 with 30% Long Carbon Fiber
Celanese Nilit FRIANYL A63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
Avient Lubri-Tech™ NN-20CF/15T Nylon 6/6, Carbon Fiber Reinforced, PTFE Lubricated
Avient Lubri-Tech™ NL-30CF/10T-2S Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated
Avient Edgetek® NN-40CF/000 Nylon 6/6, Carbon Fiber Reinforced

PFIRE4 / 38782

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.