  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin 731F Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ 731F resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This NSF/ANSI 61* listed for potable water use, FDA Food Contact compliant, injection moldable grade exhibits good surface appearance, high ductility, and good impact resistance along with low moisture absorption, creep resistance, dimensional stability, and hydrolytic stability. NORYL 731F resin is an excellent candidate for a variety of water management applications such as valves, filtration components, and water meter internals.

Features: Hydrolytic Stability,Low Creep Sensitivity

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Water Absorption 0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0600 %0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.23 %0.23 %ISO 62-1
Viscosity 9.0 cP
@Load 5.00 kg,
Temperature 280 °C
9.0 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 9.2 g/10 min
@Load 5.00 kg,
Temperature 280 °C
9.2 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength at Break 49.0 MPa7110 psi50 mm/min; ASTM D638
 51.0 MPa7400 psi50 mm/min; ISO 527
Tensile Strength, Yield 57.0 MPa8270 psi50 mm/min; ISO 527
 58.0 MPa8410 psi50 mm/min; ASTM D638
Elongation at Break 17 %17 %50 mm/min; ISO 527
 28.1 %28.1 %50 mm/min; ASTM D638
Elongation at Yield 3.5 %3.5 %50 mm/min; ISO 527
 7.2 %7.2 %50 mm/min; ASTM D638
Tensile Modulus 2.70 GPa392 ksi1 mm/min; ISO 527
 2.86 GPa415 ksi50 mm/min; ASTM D638
Flexural Strength 89.0 MPa12900 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
 90.0 MPa13100 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 95.0 MPa13800 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.42 GPa351 ksi2.6 mm/min, 100 mm span; ASTM D790
 2.55 GPa370 ksi2 mm/min; ISO 178
 2.64 GPa383 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 213 J157 ft-lbASTM D256
 133 J
@Temperature -40.0 °C
98.1 ft-lb
@Temperature -40.0 °F
ASTM D256
Izod Impact, Notched (ISO) 17.0 kJ/m²8.09 ft-lb/in²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.70 J/cm²8.09 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Gardner Impact  5.00 J
@Temperature -40.0 °C
3.69 ft-lb
@Temperature -40.0 °F
ASTM D3029
 25.0 J
@Temperature -30.0 °C
18.4 ft-lb
@Temperature -22.0 °F
ASTM D3029
Dart Drop, Total Energy 48.0 J35.4 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.65
@Frequency 50.0 - 60.0 Hz
2.65
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 21.6 kV/mm
@Thickness 3.20 mm
549 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor 0.00040
@Frequency 50.0 - 60.0 Hz
0.00040
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 250 - 400 V250 - 400 VUL 746A
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=3.00 mm
30 - 60 sec
@Thickness >=0.118 in
UL 746A
 60 - 120 sec
@Thickness >=1.50 mm
60 - 120 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
@Thickness >=1.50 mm
15 - 30 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  91.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
51.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 91.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
51.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  95.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 95.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
53.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)  131 °C
@Thickness 3.20 mm
268 °F
@Thickness 0.126 in
unannealed; ASTM D648
 137 °C
@Thickness 6.40 mm
279 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 117 °C
@Thickness 3.20 mm
243 °F
@Thickness 0.126 in
unannealed; ASTM D648
 126 °C
@Thickness 6.40 mm
259 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 140 °C284 °FRate B/50; ISO 306
 143 °C289 °FRate B/120; ISO 306
 148 °C298 °FRate B/50; ASTM D1525
UL RTI, Electrical 105 °C221 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 105 °C221 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
Oxygen Index 22 %22 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 310 °C536 - 590 °F
Zone 2 260 - 305 °C500 - 581 °F
Zone 3 270 - 310 °C518 - 590 °F
Melt Temperature 280 - 310 °C536 - 590 °FInjection Molding
Mold Temperature 75.0 - 105 °C167 - 221 °F
Drying Temperature 105 - 110 °C221 - 230 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82252 / 290199

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.