Physical Properties | Metric | English | Comments |
---|
Density | 1.19 g/cc | 0.0430 lb/in³ |
Viscosity | 177 cP @Shear Rate 206 1/s, Temperature 200 °C | 177 cP @Shear Rate 206 1/s, Temperature 392 °F |
Melt Flow | 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C | 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 28 @Time 15.0 sec | 28 @Time 0.00417 hour |
| 30 @Time 5.00 sec | 30 @Time 0.00139 hour |
| 32 @Time 1.00 sec | 32 @Time 0.000278 hour |
| 24.4 @Treatment Temp. 110 °C, Time 15.0 sec | 24.4 @Treatment Temp. 230 °F, Time 0.00417 hour |
| 24.5 @Treatment Temp. 125 °C, Time 15.0 sec | 24.5 @Treatment Temp. 257 °F, Time 0.00417 hour |
| 26.8 @Treatment Temp. 125 °C, Time 5.00 sec | 26.8 @Treatment Temp. 257 °F, Time 0.00139 hour |
| 27.9 @Treatment Temp. 110 °C, Time 5.00 sec | 27.9 @Treatment Temp. 230 °F, Time 0.00139 hour |
| 29.1 @Treatment Temp. 125 °C, Time 1.00 sec | 29.1 @Treatment Temp. 257 °F, Time 0.000278 hour |
| 70.4 @Treatment Temp. 110 °C, Time 1.00 sec | 70.4 @Treatment Temp. 230 °F, Time 0.000278 hour |
Tensile Strength at Break | 2.10 MPa | 305 psi |
| 3.30 MPa | 479 psi |
| 2.52 MPa @Treatment Temp. 110 °C, Time 3.629e+6 sec | 366 psi @Treatment Temp. 230 °F, Time 1008 hour |
| 2.73 MPa @Treatment Temp. 125 °C, Time 605000 sec | 397 psi @Treatment Temp. 257 °F, Time 168 hour |
| 5.61 MPa @Treatment Temp. 110 °C, Time 3.629e+6 sec | 814 psi @Treatment Temp. 230 °F, Time 1008 hour |
| 5.71 MPa @Treatment Temp. 125 °C, Time 605000 sec | 829 psi @Treatment Temp. 257 °F, Time 168 hour |
Tensile Stress at Strain | 0.550 MPa @Strain 100 % | 79.8 psi @Strain 100 % |
| 1.01 MPa @Strain 100 % | 146 psi @Strain 100 % |
| 0.510 MPa @Strain 100 %, Treatment Temp. 125 °C | 74.0 psi @Strain 100 %, Treatment Temp. 257 °F |
| 0.540 MPa @Strain 100 %, Treatment Temp. 110 °C | 78.4 psi @Strain 100 %, Treatment Temp. 230 °F |
| 0.805 MPa @Strain 100 %, Treatment Temp. 125 °C | 117 psi @Strain 100 %, Treatment Temp. 257 °F |
| 0.846 MPa @Strain 100 %, Treatment Temp. 110 °C | 123 psi @Strain 100 %, Treatment Temp. 230 °F |
Elongation at Break | 470 % | 470 % |
| 860 % | 860 % |
| 517 % @Treatment Temp. 125 °C, Time 605000 sec | 517 % @Treatment Temp. 257 °F, Time 168 hour |
| 935 % @Treatment Temp. 110 °C, Time 3.629e+6 sec | 935 % @Treatment Temp. 230 °F, Time 1008 hour |
| 1060 % @Treatment Temp. 110 °C, Time 3.629e+6 sec | 1060 % @Treatment Temp. 230 °F, Time 1008 hour |
| 1250 % @Treatment Temp. 125 °C, Time 605000 sec | 1250 % @Treatment Temp. 257 °F, Time 168 hour |
Tear Strength | 12.3 kN/m | 70.0 pli |
| 16.3 kN/m | 93.0 pli |
Compression Set | 15 % @Temperature 22.8 °C, Time 79200 sec | 15 % @Temperature 73.0 °F, Time 22.0 hour |
| 39 % @Temperature 70.0 °C, Time 79200 sec | 39 % @Temperature 158 °F, Time 22.0 hour |
| 71 % @Temperature 90.0 °C, Time 252000 sec | 71 % @Temperature 194 °F, Time 70.0 hour |
| 94 % @Temperature 125 °C, Time 252000 sec | 94 % @Temperature 257 °F, Time 70.0 hour |
|
Processing Properties | Metric | English | Comments |
---|
Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F |
Middle Barrel Temperature | 177 - 199 °C | 350 - 390 °F |
Front Barrel Temperature | 182 - 204 °C | 360 - 400 °F |
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F |
Melt Temperature | 188 - 210 °C | 370 - 410 °F |
Mold Temperature | 25.0 - 65.6 °C | 77.0 - 150 °F |
Injection Pressure | 1.38 - 6.89 MPa | 200 - 1000 psi |
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi |
Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in |
Screw Speed | 50 - 100 rpm | 50 - 100 rpm |
|
Descriptive Properties |
---|
Appearance | Black |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.