MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kaltun GLASSTUN FELDSPAR S.PR.600.GQ for Glass Production
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: GLASTUN feldspar is used in flat glass, container glass, architectural glass, auto glasses, technical glass (screen, etc.) solar glass, tableware and crystal glass productions. All GLASSTUN products are produced in mines belonging to Kaltun Madencilik A.S. and located in Çine-Milas region.

Information provided by KALTUN MINING

Key Words: Product Code: KSC.74.G.0600
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.60 g/cc0.0939 lb/in³
Moisture Absorption 0.200 %0.200 %
Loss On Ignition 0.25 %0.25 %
Particle Size 100 µm100 µm10% Screening (wet/dry)
 >= 100 µm>= 100 µm90% Screening (wet/dry)
 113.1 µm113.1 µmD10, Laser Diffraction - MIE (Malvern)
 249.3 µm249.3 µmD50, Laser Diffraction - MIE (Malvern)
 >= 500 µm>= 500 µm0% Screening (wet/dry)
 635.6 µm635.6 µmD97, Laser Diffraction - MIE (Malvern)
 >= 800 µm>= 800 µm0% Screening (wet/dry)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 6.06.0
 
Component Elements PropertiesMetricEnglishComments
Al2O3 19.8 %19.8 %
CaO 1.3 %1.3 %
Fe2O3 0.0275 %0.0275 %
K2O 0.25 %0.25 %
MgO 0.070 %0.070 %
Na2O 10.8 %10.8 %
SiO2 67.5 %67.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKALT840 / 318138

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.