MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Elkem (Bluestar Silicones) BLUESIL™ FLD 48 V 750 Polydimethylsiloxane Fluid
Categories: Fluid

Material Notes: Description: BLUESIL™ FLD 48V Series is a hydroxyl terminated linear polydimethylsiloxane fluid.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/cc
Viscosity 750 cP750 cP
Storage Temperature 5.00 - 25.0 °C41.0 - 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point -45.0 °C-49.0 °F
Flash Point 230 °C446 °Fclosed cup
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
Appearanceclear liquid
Hydroxyl0.0014

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ FLD 48 V 750 to 1000000 Polydimethylsiloxane Silicone Oils
Elkem (Bluestar Silicones) BLUESIL™ FLD 48 V 135000 Polydimethylsiloxane Fluid
Elkem (Bluestar Silicones) BLUESIL™ FLD 48 V 100 Polydimethylsiloxane Fluid

PBLUST112 / 191095

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.