MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hydraulic Bronze, UNS C83800, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Sand Cast

Casting Characteristics: High – Casting Yield, Effect of Section Size; Medium – Fluidity, Gassing, Shrinkage in Solidification; Low - Drossing

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing; Fair Suitability – Coated Metal Arc Welding

Typical uses: Hardware; Electrical Components; Switches; Air-Gas-Water Fittings; Bushings; Pump Fixtures; Railroad Catenary Fittings; Valves; Plumbing Fixtures

Applicable Specifications: As Centrifugal Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B271/B271M; As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – Castings SAE J462, Castings ASTM B584, Castings SAE J461, Castings B763/B763M; Fitting – ASTM B584, ASME B16.32, ASME B16.23, ASME B16.18, ASME B16.15; Ingot - ASTM B30; Unions – FEDERAL WW-U-516

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.312 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 60
@Load 500 kg
Tensile Strength >= 30.0 ksifor Standard
 35.0 ksiTypical
Tensile Strength, Yield >= 13.0 ksifor Standard, 0.5% Ext
 16.0 ksiTypical, 0.5% Ext
Elongation at Break >= 20 %for Standard
 25 %Typical
Tensile Modulus 13300 ksi
Compressive Strength 12.0 ksi0.001 in. set/in.
 29.0 ksi0.01 in. set/in.
Machinability 90 %
Izod Impact 8.00 ft-lb
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000115 ohm-cm15% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 41.8 BTU-in/hr-ft²-°F
Melting Point 1550 - 1840 °F
Solidus 1550 °F
Liquidus 1840 °F
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 500 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.25 %
Copper, Cu 82 - 83.8 %
Iron, Fe <= 0.30 %
Lead, Pb 5.0 - 7.0 %
Nickel, Ni <= 1.0 %
Phosphorus, P <= 0.030 %
Silicon, Si <= 0.0050 %
Sulfur, S <= 0.080 %
Tin, Sn 3.3 - 4.2 %
Zinc, Zn 5.0 - 8.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC83800x3 / 293147

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.