MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® HexPly® M92/48%/285H5/AS4C-3K Epoxy Matrix, AS4C-3K Carbon Fiber
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes:

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³Resin
 1.44 g/cc0.0520 lb/in³Nominal Laminate
 1.78 g/cc0.0643 lb/in³Fiber
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 782 MPa113000 psiWarp; EN2561B
Tensile Modulus 50.3 GPa7300 ksiWarp; EN2561B
Compressive Strength 573 MPa83100 psiWarp; EN2850B
Compressive Modulus 0.0404 GPa5.86 ksiWarp; EN2850B
Shear Modulus 2.70 GPa392 ksiIn-plane; EN 6031
Shear Strength 57.4 MPa8330 psiInterlaminar; EN 2563
 96.0 MPa13900 psiIn-plane; EN 6031
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 115 °C239 °FWet, DMA extrapolated onset E’; EN6032
 166 °C331 °FDry, DMA extrapolated onset E’; EN6032
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
Fabric Weight285 g/m2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9175 / 322331

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.