MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Radici Raditer® B RVA 100 Polybutylene Terephthalate with 10% Glass fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.

Information provided by Radici group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccISO 1183
Moisture Absorption at Equilibrium 0.22 %0.22 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0095 cm/cm0.0095 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 75 %75 %ISO 527-2/1A
Tensile Modulus 4.20 GPa609 ksiISO 527-2/1A
Flexural Strength 120 MPa17400 psiISO 178/1A
Flexural Modulus 3.50 GPa508 ksiISO 178/1A
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179 eU
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FISO 11357-1-3
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FISO 75-2/Bf
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FISO 75-2/Af
Vicat Softening Point 100 °C
@Load 5.10 kg
212 °F
@Load 11.2 lb
50°C/h; ISO 306/B50
Flammability, UL94 HBHB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Lupox® GP2100 PBT+GF10%
LG Chemical Lupox® TE5100 PBT+PC+GF10%
BLUESTAR PBT 6630 30% Glass Filled
BASF Ultradur® B 4040 G10 BK5110 50% Glass Filled PBT
Plastcom SLOVASTER® B GB 30 PBT, 30% glass beads

PRADI774 / 120287

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.