MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Superior Flux Superior No. 2040 Water-Soluble Tack Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Passes IPC Tests
  • Superior wetting characteristics, lot-to-lot consistency, and stable viscosity
  • No slump
  • Halide-free, halogen-free
  • Long tack time
  • Residues are completely Water-Soluble. Post-solder residues can be maintained if delayed cleaning is necessary up to 168 hours with no adverse effects on SIR Values.
  • THIS PRODUCT IS RoHS COMPLIANT.
Description: Superior 2040 Water-Soluble Tacky Flux is a Water-Soluble formulation for electronics applications requiring highreliability, stability, and cleanliness. Flux formulation contains no ionic materials and is suitable for clean-room applications.

Applications: Superior 2040 Water-Soluble Tacky Flux is formulated for BGA rework and repair, or specialty processes where a conventional flux does not provide sufficient activity and/or requires post-solder cleaning. Flux can be placed on surface area by printing, dispensing, or manually applying the flux. When cleaning all residues, a water temperature of 60ºC/140ºF is recommended for optimum results. DO NOT use isopropyl alcohol to clean post-solder residues. Residues are water-soluble. Isopropyl and other solvents will prolong the cleaning process and should not be used for residue removal or tacky flux cleaning.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 18.0 - 25.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 1.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSFLUX094 / 185778

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.