LACQTENE® 2004 TN 52 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2004 TN 52 is best processed between 190 and 230°C. Information provided provided by Total Petrochemicals. Total Petrochemicals includes former Fina and Atofina plastics product lines. |