MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik SAF 2205SH Spring Wire
Categories: Metal; Ferrous Metal; Duplex; Special-Purpose Steel; Stainless Steel

Material Notes: Sandvik SAF 2205SH is a duplex (austenitic-ferritic) stainless steel which has a very good corrosion resistance, superior to that of AISI 316. The high tensile strength make it possible to reduce the size of the wire in the springs why it is good for example component in electronics.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2092.5 - 2407.5 MPa
@Diameter 1.00 mm
 2371.5 - 2728.5 MPa
@Diameter 0.200 - 0.700 mm
Tensile Strength, Yield 1800 MPa
@Strain 0.2 %,
Diameter 1.00 mm
 2050 MPa
@Diameter 0.200 - 0.700 mm,
Strain 0.2 %
Modulus of Elasticity 200 GPaas delivered
 205 GPaas tempered
Poissons Ratio 0.30Calculated
Shear Modulus 77.0 GPaas received
 79.0 GPaas tempered
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000840 ohm-cm
@Temperature 50.0 - 100 °C
Magnetic Permeability 60µ, annealed
 120µ, cold drawn
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 100 °C
 12.8 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 19.0 W/m-K
@Temperature 300 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 22 %
Iron, Fe 67.5 %as balance
Manganese, Mn 1.5 %
Molybdenum, Mo 3.2 %
Nickel, Ni 5.2 %
Nitrogen, N 0.17 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.40 %
Sulfur, S <= 0.015 %
 
Descriptive Properties
Tempering Effect200-450 Mpa; 450°C/30 minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik 11R51 Spring Wire
Sandvik 12R10 Spring Wire
Sandvik 5R60/5R62 Spring Wire
Sandvik 2RK66 Spring Wire
Sandvik 75X1 Spring Wire

NSANDV272 / 19166

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.