MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 7868 Thermal Transfer Polyester Label Material
Categories: Polymer; Adhesive

Material Notes: 3M™ Thermal Transfer Polyester Label Material 7868 is a gloss radiant white polyester label stock that offers premium durability and moisture resistance. This label product utilizes 3M™ Adhesive 350, which is a universal adhesive for label material that offers excellent chemical resistance and holding strength even at high temperatures.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 27.9 microns1.10 milAdhesive
 50.8 microns2.00 milFacestock
 81.3 microns3.20 milLiner
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.1205 kN/m0.6875 pliLDPE, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.1205 kN/m0.6875 pliLDPE, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.131 kN/m0.750 pliPolypropylene, 90° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.1424 kN/m0.8125 pliHDPE, 90° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.20817 kN/m1.1875 pliHDPE, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.219 kN/m1.25 pliPolypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.2410 kN/m1.375 pliLDPE, 90° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.2410 kN/m1.375 pliPolypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.2410 kN/m1.375 pliHDPE, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.27391 kN/m1.5625 pliPolycarbonate, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.27391 kN/m1.5625 pliLDPE, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.27391 kN/m1.5625 pliPolypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.2849 kN/m1.625 pliHDPE, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.33964 kN/m1.9375 pliLDPE, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.33964 kN/m1.9375 pliPolycarbonate, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.36156 kN/m2.0625 pliLDPE, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.3725 kN/m2.125 pliSmooth Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.3725 kN/m2.125 pliFinely Textured Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.38347 kN/m2.1875 pliLDPE, 180° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.38347 kN/m2.1875 pliFinely Textured Powder Coating, 180° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.38347 kN/m2.1875 pliLDPE, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.394 kN/m2.25 pliFinely Textured Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.394 kN/m2.25 pliPolypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.40538 kN/m2.3125 pliHDPE, 180° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.42729 kN/m2.4375 pliHDPE, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.42729 kN/m2.4375 pliHDPE, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.438 kN/m2.50 pliHDPE, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.44921 kN/m2.5625 pliPolypropylene, 180° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.5040 kN/m2.875 pliPolycarbonate, 90° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.51494 kN/m2.9375 pliStainless Steel, 90° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.5478 kN/m3.125 pliPolypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.5478 kN/m3.125 pliPolypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.570 kN/m3.25 pliPolycarbonate, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.58068 kN/m3.3125 pliPolycarbonate, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.5916 kN/m3.375 pliPolycarbonate, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.66833 kN/m3.8125 pliGlass, 90° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.701 kN/m4.00 pliFinely Textured Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.71216 kN/m4.0625 pliSmooth Powder Coating, 180° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.7231 kN/m4.125 pliSmooth Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.745 kN/m4.25 pliGlass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.75598 kN/m4.3125 pliGlass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.7669 kN/m4.375 pliPolycarbonate, 180° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.77789 kN/m4.4375 pliSmooth Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.789 kN/m4.50 pliStainless Steel, 180° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.79981 kN/m4.5625 pliStainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.8108 kN/m4.625 pliGlass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.82172 kN/m4.6875 pliGlass, 180° Peel, Initial, 10 min Dwell RT; ASTM D3330
 0.82172 kN/m4.6875 pliPolycarbonate, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.877 kN/m5.00 pliGlass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.88746 kN/m5.0625 pliGlass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.88746 kN/m5.0625 pliStainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 0.90937 kN/m5.1875 pliStainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 0.90937 kN/m5.1875 pliStainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.920 kN/m5.25 pliGlass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.964 kN/m5.50 pliStainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 1.01 kN/m5.75 pliStainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= -40.0 °C>= -40.0 °FApplication
 <= 149 °C<= 300 °FApplication
 
Descriptive Properties
Adhesive Type#350 Acrylic
Liner55# Densified kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34264 / 169011

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.