MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol ESTANE® X4985 Ether Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.

Benefits of Estane® TPU:

  • Outstanding Abrasion and Wear Resistance
  • Excellent Low Temperature Flexibility
  • Superior Toughness and Durability
  • Ease of Processing and Manufacturing Flexibility
  • Colorability and Paintability with no adhesion promoter
  • Applications:

    • Film & Sheet
    • Fabric coating & melt coating
    • Wire & Cable
    • Hose, Tube & Profile
    • Custom molding
    • Custom compounding
    • Automotive interior/chassis and exterior painted trim

    Information provided by Noveon, Inc.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.14 g/cc1.14 g/ccDIN 53479
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore D 4545DIN 53505
    Tensile Strength, Ultimate 38.0 MPa5510 psiDIN 53504
    Elongation at Break 550 %550 %DIN 53504
    50% Modulus 9.20 MPa
    @Strain 50 %
    9.20 MPa
    @Strain 50 %
    DIN 53504
    100% Modulus 10.8 MPa
    @Strain 100 %
    1570 psi
    @Strain 100 %
    DIN 53504
    300% Modulus 18.8 MPa
    @Strain 300 %
    2730 psi
    @Strain 300 %
    DIN 53504
    Flexural Stiffness 49.00 MPa7107 psiASTM D747
    Tear Strength 100 kN/m571 pliDIN 53515
    Abrasion 6666mm3; DIN 53516
     
    Thermal PropertiesMetricEnglishComments
    Vicat Softening Point 85.0 °C185 °FA50; DIN 53460
     
    Descriptive Properties
    E-Modulus47 mm/min

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
    Huntsman IROGRAN® A 92 P 4207 TPU-Polyether
    Covestro Texin® DP7-1049 Thermoplastic Polyurethanes (TPU)
    Covestro Baytec® ME-120 Polyurethane
    Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System

    PNOVEON181 / 55452

    Polyurethane

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.