MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV X6180N Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV X6100 series are engineered materials designed for consumer, automotive, and industrial applications requiring superior Colorability and elastic performance. This product is a medium hardness, low density, multi-purpose thermoplastic vulcanizate that does not require pre-drying and can be processed by injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Flow; Good Processability; Medium Hardness; Low Density; Low Specific Gravity; Resilient

Uses: Automotive Applications; Automotive Interior Parts; Consumer Applications; Industrial Applications; Rubber Replacement; Soft Touch Applications

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.973 g/cc0.0352 lb/in³ISO 1183
Viscosity 212 cP
@Shear Rate 206 1/s,
Temperature 200 °C
212 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ISO 11443
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  80
@Time 5.00 sec
80
@Time 0.00139 hour
Extruded; ISO 868
 84
@Time 5.00 sec
84
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 7.31 MPa1060 psiFlow; ISO 37
 8.00 MPa1160 psiAcross Flow; ISO 37
Tensile Stress at Strain  4.20 MPa
@Strain 100 %
609 psi
@Strain 100 %
Across Flow; ISO 37
 6.00 MPa
@Strain 100 %
870 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 390 %390 %Flow; ISO 37
 650 %650 %Across Flow; ISO 37
Tear Strength 45.6 kN/m260 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  39 %
@Temperature 22.8 °C,
Time 79200 sec
39 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 54 %
@Temperature 70.0 °C,
Time 79200 sec
54 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 81 %
@Temperature 125 °C,
Time 252000 sec
81 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Descriptive Properties
AppearanceNatural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1219 / 237710

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.