Description: H 401 is a medium melt flow rate homopolymer polypropylene, additived with slip and antiblocking agents. Designed specially for cast film. This product features good impact strength, excellent transparency and gloss, good slipping and outstanding weldability. Applications: Coil for automatic packaging; Packages for food and textile products. Information provided by Braskem |