MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Lotte Advanced Materials Infino® ASF-9860 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Automotive

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ASTM D792
Water Absorption 0.400 %0.400 %ASTM D570
Melt Flow 74.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
74.0 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 85.085.0ASTM D785
Hardness, Rockwell R 116116ASTM D785
Tensile Strength at Break 44.1 MPa6400 psi5 mm/min; ASTM D638
Tensile Strength, Yield 55.9 MPa8110 psi5 mm/min; ASTM D638
Elongation at Break 30.0 %30.0 %5 mm/min; ASTM D638
Tensile Modulus 2.30 GPa334 ksi5 mm/min; ASTM D638
Flexural Strength 83.4 MPa12100 psi5 mm/min; ASTM D790
Flexural Modulus 2.60 GPa377 ksi5 mm/min; ASTM D790
Izod Impact, Notched  0.294 J/cm
@Thickness 3.17 mm
0.551 ft-lb/in
@Thickness 0.125 in
ASTM D256
 0.343 J/cm
@Thickness 6.35 mm
0.643 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
@Thickness 6.40 mm
356 °F
@Thickness 0.252 in
ASTM D648
Shrinkage, MD 0.0150 - 0.0180 %
@Thickness 3.20 mm
0.0150 - 0.0180 %
@Thickness 0.126 in
ASTM D955
Shrinkage, TD 0.0170 - 0.0200 %
@Thickness 3.20 mm
0.0170 - 0.0200 %
@Thickness 0.126 in
ASTM D955

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOTT9411 / 325893

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.