MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TSRC T-BLEND® 4003-75N-S TPR/TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: T-BLEND® is a series of thermoplastic elastomer compound materials produced by TSRC (Shanghai) Industries LTD. T-BLEND® 4003-75N-S is specially designed for replacing conventional foaming elastomer such as EVA/POE, and it can be used as modifier for EVA and POE foaming. T-BLEND® 4003-75N-S has excellent elasticity, flexibility and fine cells.

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 - 1.10 g/cc1.06 - 1.10 g/ccASTM D792
Melt Flow 3.0 - 9.0 g/10 min
@Load 5.00 kg,
Temperature 180 °C
3.0 - 9.0 g/10 min
@Load 11.0 lb,
Temperature 356 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 73 - 7973 - 79ASTM D2240
Tensile Strength 2.94 MPa427 psiType3, specimen; ASTM D412
Elongation at Break 250 %250 %Crosshead; ASTM D412
Tear Strength 19.6 kN/m112 pliC Die; ASTM D624
 
Processing PropertiesMetricEnglishComments
Drying Temperature 50.0 °C
@Time 3600 - 7200 sec
122 °F
@Time 1.00 - 2.00 hour
hot air circulating oven/hopper
 
Descriptive Properties
ColorNatural
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTSRC068 / 306356

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.