105°C, VW-1 rated non-lead stabilized insulation compound. Ideally suited for 18 AWG, 1/64 wall. UL approved for TW, THW, THHW applications. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |