MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Lupolen 2420F PLUS Low Density Polyethylene (LDPE), Blown Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Lupolen 2420 F PLUS is a non-additivated, low density polyethylene. This grade is characterized by a very low gel level. Typical customer applications are surface protection films or other higher value film applications where a very low gel content is required . It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications: Bags & Pouches, Food Packaging Film, Hygiene Film, Liner Film, Shrink Film, Surface Protection Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ISO 1183-1
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 11.0 MPa1600 psiISO 527-1,-2
Film Elongation at Break, MD 300 %300 %ISO 527-1,-3
Film Elongation at Break, TD 600 %600 %ISO 527-1,-3
Tensile Modulus 0.260 GPa37.7 ksiISO 527-1,-2
Coefficient of Friction >= 0.80>= 0.80ISO 8295
Dart Drop Test 150 g0.331 lbF50; ASTM D 1709
Film Tensile Strength at Break, MD 26.0 MPa3770 psiISO 527-1,-3
Film Tensile Strength at Break, TD 24.0 MPa3480 psiISO 527-1,-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 111 °C232 °Fpeak; ISO 3146
Vicat Softening Point 96.0 °C205 °FA50N; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 8.0 %
@Thickness 0.0500 mm
<= 8.0 %
@Thickness 0.00197 in
ASTM D1003
Gloss >= 40 %>= 40 %@ 20°; ASTM D2457
 >= 90 %>= 90 %@ 60°; ASTM D2457
 
Descriptive Properties
Failure Energy (J/mm)5.5DIN 53373
Processing MethodBlown Film
Test Specimenfilm, 50µm blown film extruded at 180°C, and a blow up ratio 2.5:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 2420F Low Density Polyethylene (LDPE), Blown Film Grade

PEQT8531 / 220166

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.