MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Baytec® 33965-1 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Baytec 33965-1 is a moldable polyurethane elastomer system.

Properties / Applications: Baytec 33965-1 is a filled elastomer system developed for pool and spa applications. This system can be used to encapsulate filter media by casting fully structural end-caps. Baytec 33965-1 forms a tough, durable elastomer with excellent impact resistance and a hardness of 80 Shore D. Parts made with Baytec 33965-1 also have excellent resistance to common pool and spa chemicals. As with any product, use of Baytec 33965-1 system in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.205 - 1.23 g/ccRX-32086-B PREPOLYMER (Component A)
 1.205 - 1.23 g/ccBAYTEC 33965-1 (Component B)
Viscosity 650 - 1050 cPRX-32086-B PREPOLYMER (Component A)
 990 - 1220 cPBAYTEC 33965-1 (Component B)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 77 - 85
 
Processing PropertiesOriginal ValueComments
Gel Time 2.75 - 3.25 min
 
Descriptive Properties
AppearanceBlack liquidBAYTEC 33965-1 (Component B)
 Clear to hazy amber liquidRX-32086-B PREPOLYMER (Component A)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BCC Products BC 8165 Urethane Casting
BCC Products BC 8782 Urethane Casting
BCC Products Kwik Kast BC 8001 Urethane Casting
BCC Products Kwik Kast BC 8002 Urethane Casting
BCC Products Proto-Kast BC 8163 Urethane Casting

PCOVEST0232 / 202015

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.