MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Proto3000 Objet TangoBlackPlus FullCure980 Rubber-like Prototyping Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid Prototyping and Rapid Manufacturing applications.

Tango Family: Rubber like flexible materials with various levels of elasticity

Fields of Use: Consumer goods, Toy, Telecommunications, Computers and Architecture fields, Jewelry applications

Information provided by Proto3000 for their protoyping engineering services.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.12 - 1.13 g/ccPolymerized; ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 26 - 28ASTM D2240
Tensile Strength at Break 0.800 - 1.50 MPaASTM D415
Elongation at Break 170 - 220 %ASTM D415
Tear Strength 2.00 - 4.00 kg(f)/cmASTM D624
Compression Set 4.0 - 5.0 %ASTM D395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3D Systems Accura® 60 Plastic for SLA® Systems
3D Systems Accura® 55 Plastic for SLA® Systems
DSM Somos® ProtoGen™ 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DSM Somos® ProtoGen™ 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC +3
DSM Somos® ProtoGen™ 18420 Epoxy Resin for Stereolithography, UV & Thermal Postcure

PPROTO940 / 133142

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.